50’s 16” Yates American jointer

4/21/25       
Dave Mayer

Website: http://MC3 millworks

How do I set spring joint lever. Having trouble getting a straight joint. I don’t want a spring joint.

4/23/25       #3: 50’s 16” Yates American jointer ...
Dustin Orth

I had a Northfield that had that same ability. The infeed and outfeed tables must be parallel with each other to avoid spring joints. I used a long straight edge and set the infeed at 0. Then set the straight edge on the out feed and bridge to the infeed. Adjust the outfeed table until its perfect with the infeed. Then check the cutterhead to make sure its lined up with the outfeed table. Don't forget to check at the left side and right side of the cutterhead to make sure the tables are not set at a twist. Hope this helps.

4/30/25       #6: 50’s 16” Yates American jointer ...
BH Davis  Member

Website: http://www.bhdavis.net
As long as the tables are true to one another as explained above the next most important setup detail is cutter head to outfeed table alignment. The top of the cutters MUST be both perfectly parallel to the width of the outfeed table and perfectly even with the outfeed table surface when at the high point of the cutting arc.

You need to set the knives so they are parallel with the table surface. Then you need to adjust the height of the outfeed table to match the high point of the knife swing.

If the outfeed table is lower than the cutter head high point you will not get a straight cut.

If the outfeed table is higher than the cutter head high point the lead end of your board will butt into the end of the outfeed table.

In my opinion the two most difficult machines to set up properly in the average woodshop are the band saw and the jointer. Both need to be in correct alignment in order to work correctly.

BH Davis
5/4/25       #7: 50’s 16” Yates American jointer ...
Karl E Brogger  Member

Website: http://www.sogncabinets.com

Cutter elevation can be set close with the machine off, but in my experience needs to be dialed in while the machine is running. The head doesn't sit in the same spot at zero rpm as it does at operational speed.

5/11/25       #8: 50’s 16” Yates American jointer ...
David R Sochar Member

Here is how I set up a joiner:
a 1" x 2" x 12" S4S straight hardwood block or similar is needed. Set the new knife a bit too high (1/8" +/-) in the slot and lightly snug the retaining bolts at either end. Use a urethane hammer or block of wood to tap the knife down until it is parallel with outfeed table. Place the hardwood block on the outfeed table at the end of the knife nearest you. Slowly move the head back and forth until it lifts the block and drags it about 1/8". Snug the bolt a bit more, and move to the far end. Repeat the setting and snugging of the bolt.
Now, use the hardwood block or urethane hammer to tap the knife down a bit. Since you may be moving the knife in very small dimensions, place a finger on the knife and the head so you can detect movement. Keep tapping down on one end and the other until the hardwood block on tho outfeed table is lifted and moved about 1/32". A bit of snugging the retainer bolts is required here. Mark the block with a pencil even with the outfeed table edge , and the same at the finish position. Once they are moving the block 1/32", tighten all the retaining bolts. Do this on all 3/4 knives. Now, we have all knives set into the same arc, and parallel with the outfeed table. Drop the outfeed table so you are well below the cutterhead Top Dead Center, 1/8" or so. Then carefully raise it until your hardwood block, with the weight of your hand on it, moves just a hair. The width of the pencil line works for me. Check all the retainer bolts on every knife before powering on. Now, run a light joint on two 4 foot pieces of hardwood, and inspect the mating of the two. If hollow or end sprung, adjust the out feed carefully. A few thousandths are huge at this point. There should be no end snipe or the table is too low. The joint should not 'run out' - go from full depth cut at the start, to nothing - no cut - along the board. This indicates the table is too high.

A word about threaded adjustments. If you have ever turned a guitar or any stringed instrument you know to go below the likely final position and come up to the proper setting. This keeps the tension even and strong on every string. The tables on many joiners are moved by threaded rods, so they also need to be treated as the instruments. Take the setting well below where you want to be, and come up on it. If there is any lash or play in the system, this overcomes it and will provide a stable depth setting.   

This sounds complicated, and first time will be slow and tedious.   Once you get the hang of it, it is like second nature.

1/27/26       #9: 50’s 16” Yates American jointer ...
JamesS53 Member

Good advice above. On those older Yates machines the spring joint usually isn’t the lever itself, but table alignment. Once the infeed and outfeed are truly coplanar and the knives are set dead flush with the outfeed, the spring joint function effectively disappears.

I’d also add: double-check with a straightedge diagonally corner to corner, not just front to back. Those big cast tables can be sneaky if there’s even a slight twist. Once it’s dialed in, those old Yates jointers will cut dead straight all day.

1/27/26       #10: 50’s 16” Yates American jointer ...
David R Sochar

Northfield and others made a grinder that registered on the offend side of the pointer and ground the knives dead parallel to the outfield.
There also were some stone holding jigs that would touch the knives under power to make them parallel. These jointed knives greatly increased the noise level of a jointer, so use hearing protection.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!