Veneer

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Does 10mil paperbacked veneer protect mdf substrate?

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Does 10mil paperbacked veneer protect mdf substrate?

9/4/13       
antonio

This is my first time using MDF as a substrate to do a whole kitchen that calls for 10mil paperbacked anigre veneer. I got a lot of mixed feedback using mdf,,, moisture issues mainly. Just wondering,, if the mdf is being laminated with veneer, then sealed then top coated with clear conversion varnish,, wont that go very far in keeping moisture from the mdf?

9/5/13       #2: Does 10mil paperbacked veneer prote ...
JeffD

Not so much. A good finish will slow down the transfer of moisture, but will not prevent it. The veneer is simply wood, so that won't prevent transfer either. I'm don't use mdf for boxes as I find it's just too difficult to deal with. Even when properly pre-drilled it can still split if your not careful with fasters. Plus it's heavy as hell to move around! It's good for doors and even panels, but I just avoid it when it comes to boxes.

Normally on a kitchen you would not veneer the boxes anyway. You would band the faces and end panels, but the interiors could still be pre-finished maple or melamine. Of course if you have the budget to veneer the whole thing then by all means, that'll make for some very expensive interiors;>)

good luck,
JeffD

9/5/13       #3: Does 10mil paperbacked veneer prote ...
antonio

thanks jeff, sorry i was a bit vague. By saying i wwas doing a whole kitchen with 10mil paperback veneer, i only meant the doors. all my boxes are 3/4" birch ply, laminated one side with plastic laminate. just trying to be confident that my doors wont swell up anytime soon by using mdf as a sub.

9/5/13       #4: Does 10mil paperbacked veneer prote ...
Gerry

My kitchen has about 20 veneered MDF doors, and they are perfectly fine after about 10 years. I used plain veneer, though, not paperback.

9/5/13       #5: Does 10mil paperbacked veneer prote ...
rich

In another post on this continuing saga of paperbacked you make this comment.
"#6: Do both sides of panels have to be ...
antonio

thanks rich, i totally agree with you. The other reason why i started having second thoughts about edgebanding first was i realized that no matter how tight i press the veneer with cauls/platens etc , some of the edges always seem to not stick well,, ,maybe like up to 1/4" back from the edge or so. So i figure, glue up the panel about 1" bigger to allow for those lose edges, then cut back to where i know its glued tightly. Btw, im using that pink FSV glue on 10mil paperbacked veneer to an MDF sub. "

But now you think the edgebanding will be really nice and tight and a coat of finish will seal it just fine. Which is it?
Guing anything to the edge of mdf is problematic, let alone a piece of paper with paper thin veneer stuck to it. I say you're in for trouble in a year or so. Better put a short warranty on this job!

Different rich by the way for the quote.

9/5/13       #6: Does 10mil paperbacked veneer prote ...
antonio

Rich, i have no idea what you just did there. Sorry it was a long day at work for me and im lost as to what you are talking about. But in my previous post about the ''edges & edgebanding'' had nothing to do with me questioning whether or not i thought paperback veneer would stick to the edges of the mdf... the ''edges'' i was referring to are the face and back of the door closer to the ends. If you will,, when you press a piece of veneer to the face of a substrate, the outer edge of that face was a bit problematic at first,,, after clamping for hours it would still be easy to pull off,,, i realized i didnt have enough cauls on it,,, after adding more cauls,, problem solved. But seeing that you thought i was referring to edges (where the edgebanding goes) ,,, how else would you cover those ? if not with the same veneer that goes on the face/back??

9/6/13       #7: Does 10mil paperbacked veneer prote ...
Gerry

I use 1/8" hardwood for all my door edges.

9/6/13       #8: Does 10mil paperbacked veneer prote ...
JeffD

Haven't had any problems gluing banding to the edges of mdf or melamine coated PB anymore than I have problems gluing to veneer core. Since this is basic procedure used by tens of thousands of shops across the world I'd think we'd know by now if banding mdf was a problem?

Anyway as long as your veneer is well glued and your seams are tight and sanded well, including breaking the edges so the finish will stick, you shouldn't have any moisture issues with your doors.

JeffD

9/6/13       #9: Does 10mil paperbacked veneer prote ...
rich

go ahead and use the mdf for your doors, it will be ok. I've done many tests over the years with different substrates , I actually soak the hell out of them, I've even put veneered panels out in the parking lot and let mother nature give it her best shot. As long as you have a good glue line you shouldn't have any issues.

9/7/13       #10: Does 10mil paperbacked veneer prote ...
Rich C.

Adding a C. to my name since we had two rich's adding comments.
rich,
In all your environmental testing, did any of it include paper backed veneer and FSV glue? I would be worried about edge banding with that stuff since Antonio may just be hammer veneering the edge banding in place. He's been all over the place on this one, so I have no idea how he will be applying the edge banding. If he was applying standard veneer with an edgebander, I say no problems either. But, he has no equipment and looking for "garage woodworker" methods of veneer application.
Antonio,
I was referring back to another post in this veneering saga about your doubts with veneer application. I guess I didn't see where you had corrected with a different platen and clamp set up. I still don't like paper backed as edge banding. It's just too thin and fragile in my book. I've always done work for families, and a kitchen can really take some kid abuse. Especially silverware drawers and the always denied but never eliminated junk drawer. As mentioned by another, I always edge band with solid hardwood.

9/7/13       #11: Does 10mil paperbacked veneer prote ...
antonio

For edgebanding i am using the same 10mil paperbacked veneer and fsv glue clamped to the mdf with clamps and cauls. So far so good, after letting the ones we have done already cure for 24 hours, trimmed them and sanded them with a slight round on the edges, the glue lines are very tight, and as a plus, i was worried that by edgebanding last there was going to be an evident seam or evidence of cross grain, there was none of that. Thanks guys! and we still are going to invest in the vac. press for future work,, if not even sooner.... so no more ''garage'' workshop :)

9/8/13       #12: Does 10mil paperbacked veneer prote ...
Rich

To be perfectly honest with you, I do not recommend paper backed veneer on any product. I actually used to make paper backed veneers for many different customers. The procedure for producing paper backed veneers is very ,how can I say this , tricky.If your heat, pressure and time is off even the slightest in any one of these areas, DE-LAM. Not to mention, you never get a smooth look with paper back.I would estimate about 75% of de-lam issues are actually between the paper and veneer, not the paper back and the substrate. I get the point that not everyone cannot afford a press and you're trying to work within a budget, but when it comes to paperback it's a shot in the dark. Sad to say, but that's what our trade has evolved or should I say regressed to, cheaper, faster to get materials. All I can say is follow your glue specs guidelines, think it through and try to figure out what works best for you.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)