Veneer

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Glueing up Veneer

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Glueing up Veneer

12/2/20       
TonyK. Member

Another question, Being new to veneering, I have read many articles in woodworking magazines and most say to either use a veneer press or vacuum system to press down the veneer. but one article said you can wet the veneer, then roll glue on the veneer & substrate, let it sit for an hour the "iron" on the veneer. Will this work??

12/2/20       #2: Glueing up Veneer ...
Tom Gardiner

How big are the pieces you intend to veneer? If they are large (I wouldn't iron veneer more than 2' x 2') then I wouldn't recommend the iron method. As soon as you dampen veneer with moisture in the form of water or waterborne adhesive it will curl and become hard to handle. Paper backed veneer is easier to work with this method.
Not all PVA glue is heat resetable. Do some tests to get your technique down and see if your glue will work. I have thinned Titebond a bit to lay a thinner coat on the veneer and substrate. When done right the bond is as good as a press applied one.

12/3/20       #3: Glueing up Veneer ...
ExPat Member

+1 on the small pieces, I wouldn't try it on anything large. Also, depending on the species and how wet it gets, the iron can dry out the veneer so fast that it cracks along the grain lines. I haven't seen it happen often, but I have seen it happen.

12/3/20       #4: Glueing up Veneer ...
John Van Brussel Member

Website: http://www.veneersystems.com

This method is not the best. White glues are an evaporative cure glue and the best glue line is the first cure. Drying and reacitvating these types of glue with heat weakens the glue strength by 50%. Some issues when you are doing larger pieces is how long to do you keep the iron in one place, how do you get consistent, equal pressure and what type of pressure are you actually getting.

12/3/20       #5: Glueing up Veneer ...
Tom Gardiner

Yes a lot of things can go wrong: too much glue leaving pockets of glue, too little leaving bubbles, too hot an iron will discolour the veneer and degrade the glue,etc.
On the other hand the technique allows you to apply edge veneer to curved surfaces and veneer to assembled components where it would be otherwise impossible.
It isn't an alternative to proper pressing but a good arrow in your quiver. I have had good success with it. My mantle has a decorative geometric patterned veneer edge that has stood up for a dozen years of fireplace heat with no adverse effects.

12/3/20       #6: Glueing up Veneer ...
TonyK. Member

Thanks for all the advice. It gives me more confidence before I tackle all the projects. But now another question..... In cherry, it developes a nice patina as it ages on furniture. Will a veneer do the same thing?? as I will be using solid wood in some places & veneered in others and I want hem to match as it ages.

12/3/20       #7: Glueing up Veneer ...
ExPat Member

The short answer is yes, it will patina. I commonly used veneered panels in 5-piece doors and both would change color. There may be a bit of variance in the rate of change but I am not certain of that. I have noticed it some, but that could be all the veneer came from one tree and the solid came from many different trees. Each piece of wood reacts slightly differently.

12/4/20       #8: Glueing up Veneer ...
rich c

One of the issues of that iron on is that the PVA will curl the veneer because of all the water absorption on one side of the veneer. Veneer will always be a slightly different color because of the steam and water soak before the veneer peeling and because of knife checking in the peeling procedure. Clear coat only doesn't show as much difference as dye staining.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!