Subject: Re: Veneer Dining Table Finishing options

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Veneer Dining Table Finishing options

12/30/23       
WestWD2021 Member

Hey guys, I’m working on a dining table for a client. Solid walnut, finished thickness 2.25”, double bullnose bent lam edging. Total surface size: 42”x90”x2.5”

My issue is that the client has chosen a walnut burl veneer for the top. It’s a 22mil BFV from Oakwood Veneers and they want a “natural finish”. Everything online points to the darlings of the day: Rubio and Osmo. Neither of these hard wax finishes are going to stand up to the every day abuse of a dining room table. The client does have kids. Any suggestions on a satin/natural looking finish that can take a bit of a beating? The plan is custom-made tabletop pads to cover the table for every day use but with kids you just never really know.

The 4 x 8 sheet of veneer costs about $1k so it’s something that definitely needs some consideration. Any options/suggestions are much appreciated.

12/31/23       #3: Veneer Dining Table Finishing optio ...
Dave Edgerton  Member

Ok so first each of those things contradicts i cannot understand if its solid wood with a veneer? Dont understand the construction but nonetheless you will have to go back to the customer and explain each of the options of finish and thier limitations. Sounds like you are the one who will be schellacked once the finish fails.

1/3/24       #4: Veneer Dining Table Finishing optio ...
RichC

Putting veneer on a solid walnut table will be a disaster since solid wood expands and contracts.

1/3/24       #5: Veneer Dining Table Finishing optio ...
WestWD2021 Member

@RichC Seeing as examples of veneered furniture from 200 years ago are still available I’d say that there shouldn’t be problems. Assuming the stock has been sufficiently dried and acclimated to the moisture of the space, as well as milled and glued correctly, veneer on solid wood substrate is perfectly viable. Additionally, the question was about recommended finishing options such as CV, hard wax, etc so posts such as this do nothing for the thread.

If you have suggestions about finishing, I’d be happy to hear.

1/4/24       #6: Veneer Dining Table Finishing optio ...
Nacho

If you're looking for suggestions regarding the finish I would post your inquiry in the finishing section.

1/5/24       #8: Veneer Dining Table Finishing optio ...
RichC

West, you posted in the veneer section, so I assumed it had to do with veneer. 200 years ago there were no central furnaces and wind blew through houses. Also solid wood from that time period was old growth and a lot different characteristics. You don't have to listen to my 51 years of woodworking experience, you can let the customer tell you how to do woodworking, but I think I have more experience than they do.

1/13/24       #9: Veneer Dining Table Finishing optio ...
The MW Studio Sponsor - The Millwork Studio

Website: themillworkstudio.com

Considering the delicacy of walnut burl veneer, have you thought about trying a conversion varnish? It's known for being durable and resistant to wear and tear, making it a solid choice for a high-traffic area like a dining table. The satin finish could maintain that natural look you're going for.

Another option worth exploring could be a water-based polyurethane with a satin sheen. It tends to be clear and should help preserve the natural beauty of the walnut burl while providing the necessary protection.

I totally understand the unpredictability of kids, and having custom-made tabletop pads is a smart move for daily protection. But having a finish that can hold its own is equally crucial.

Best of luck with your project, and I hope the finish you choose does justice to that gorgeous walnut burl veneer!

1/24/24       #10: Veneer Dining Table Finishing optio ...
BH Davis  Member

Website: http://www.bhdavis.net

Watco oil is a possibility. My choice would likely be that or a oil based varnish. I have used catalyzed water based finishes on cabinets successfully but don't think I'd try that on a table top.

Also, like you, I see now problem with veneer on solid wood. It has been done for hundreds of years and those pieces are surviving in modern heated/air conditioned buildings. I've done it myself.

BH Davis

2/10/24       #11: Veneer Dining Table Finishing optio ...
Oth

If they want a "natural" finish, whatever that means it'll come with all the natural issues of wear and tear. 2k poly or bust imo. Used water based and maybe that will pass for "natural". Or go squeeze some lac beetles by hand haha. At a certain point you have to steer the client to the obvious best course and not let them dictate areas of the job they may be misinformed about. Most finishes are inert once they've cured- that's probably all they're worried about with their kids. Good luck and this does belong in the finishing section.

4/11/24       #12: Veneer Dining Table Finishing optio ...
David

It would work but you have to have to have the walnut veneer two plied. We did it for years. The two ply would lessen the solid moving the veneer face. Otherwise, I can hear the checking from here.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!