Is this a balanced panel?

2/24/24       
Tim Member

We often make veneered cabinet fronts with raw veneer on front and back on an MDF substrate. I’m wondering if anyone has insight as to wether or not we could use a paper backed veneer on the back (to save time) and the raw veneer on the front?
Does the paper backing count as a layer? I assume it would.
I was thinking of going about it like this. Paper backed veneer on the back, then paper backer such as GatorPly on the face, raw face veneer over that. This way both faces have the paper underlayment. Does anyone have experience making panels this way?

2/27/24       #3: Is this a balanced panel? ...
The MW Studio Sponsor - The Millwork Studio

Website: themillworkstudio.com

Considering the requirement for the backer to be the same thickness as the face panel, you might want to explore alternatives that maintain uniformity. One option could be using a veneer with a paper backing that matches the thickness of your raw veneer on the front. This way, you achieve the desired consistency without compromising structural integrity.

2/28/24       #4: Is this a balanced panel? ...
tom gardiner

I have done this with good results. In my experience, if you are going to have issues with warping of veneered panels it will show itself in the shop in the first few days. How you handle to sheets after pressing is the most important ingredient to success.

2/28/24       #5: Is this a balanced panel? ...
Tim Member

Thanks for the replies. We’ll hot press at 90dg Celsius for 90 seconds and dead stack overnight while things cool. We’ll probably do a couple sessions of pressing in short order since we can’t do it all in one press cycle.

2/28/24       #6: Is this a balanced panel? ...
Tim Member

Ditto on the warped panels, they do tend to warp in a day or two if something is off.
2/28/24       #7: Is this a balanced panel? ...
Bozzy Member

Tim,

How thick is your raw veneer?

2/29/24       #8: Is this a balanced panel? ...
Tim Member

We haven’t purchased yet, but standard thickness .02”-.024”. Likely from Dooge or Certainly Wood.

3/9/24       #9: Is this a balanced panel? ...
David R Sochar Member

I will say no, it is not a balanced panel. Same veneer two sides is the sure thing.
Are you a gambler?
If you are 8" x 8" panels you may be able to get away with the paper. But anything larger is risky.

3/9/24       #10: Is this a balanced panel? ...
Tim Member

David,
Both sides will be a walnut veneer of the same thickness. Only difference is one side is a purchased paper backed 4x8 sheet, while the other is raw veneer over a paper backer that we lay up in house.
Do you still think that’s too much of a gamble?
I appreciate the insight.

3/10/24       #11: Is this a balanced panel? ...
David R Sochar Member

I understand the desire to save time (one pressing vs two?), but you are making what becomes a five ply panel. It does appear to be stable and balanced. Except for the fact that you will be adding two layers of glue to one side of the center, and only one layer of glue on the other side. And none of what you are adding is cross grain, to make a true plywood panel, and make it a stabl pand$

Again, if the panels are smaller and are well supported, that is different from large, and getting its flatness from some sort of trim.
I think I would take the safe route, and learn how to do a five ply glue up.

4/11/24       #12: Is this a balanced panel? ...
Jeff Member

Website: https://virmer.com/

A properly executed glue-up distributes adhesive evenly, maintaining balance and stability. Additionally, while cross-grain layers enhance stability in traditional plywood, alternative methods can achieve comparable results, especially in smaller, well-supported panels. Flexibility in approach can lead to efficient and effective outcomes without compromising quality.

4/11/24       #13: Is this a balanced panel? ...
David R Sochar Member

Jeff - You should get a gig impersonating an AI computer.

Lots of words, and you said….what?

Yes, cross grain does make plywood stiffer - it is what makes plywood plywood. I an unsure what else you said, but I did recognize a few words.

Clarification of a less confabulatory nature would add to the conversation.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!