Wood NetWork

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: blade sharpenings

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

blade sharpenings

6/11/15       
Cabmaker Member

We use a Leuco hollow ground blade for cutting on a Holzher panel saw. My question is 2 parts. 1. How many panels should we expect to cut clean (on the grid side) before a blade change (3/4" melamine), and how many sharpenings should we expect to get out of each blade? Thanks

6/13/15       #2: blade sharpenings ...
Bruce H

I think It depends on the material core, pine being easier to cut than fir. Sometimes we get two hours on a blade and sometimes a week. Cutting anything other than melamine with the blade seems to reduce the melamine cut. We always change the blade when changing material. I usually have several hollow ground blades in service at the same time. The newest one for cuts that matter two sides and a more used blade for cuts that only one side matters. I have a Striebig and changing blades isn't all that tough. I think the hardest thing about hollow ground blades is getting them serviced correctly.

6/18/15       #3: blade sharpenings ...
Cabmaker Member

Thank you Bruce. I appreciate your response.

6/18/15       #4: blade sharpenings ...
Mark V.

I have had very poor results with Leuco and other hollow ground and blades on a Striebig Compact (250 mm blades). They are expensive to buy, expensive to sharpen and don’t last very long. If I could get a dozen sheets of melamine chip free on the frame side, that would be a lot. And I don’t have to tell you, but once you have chipping on that side, the blade is done for melamine. I added scoring and now use triple chip blades and get much better blade life and no chipping on the frame side after dozens of sheets.

I can confirm what Bruce said about getting them serviced and what to cut. I have been told that not everyone can sharpen them correctly. I sent mine to Forrest Manufacturing and assumed that they knew what they were doing. Also, never cut anything other than melamine until they start chipping on the frame side.

I hope this helps.
Mark

6/19/15       #5: blade sharpenings ...
Cabmaker Member

Thanks Mark. All these responses are helpful as I think our shop is a "victim" of a salesman's false promises. We have a new Holzher panel saw (8 months old) in a shop with little manufacturing experience. Their expectations (as told by the salesman as recently as 2 weeks ago) was they should be able to cut 50 to 100 sheets of melamine and get a clean cut on the frame side even with a dull blade! Exact words. I thought that was insane and as I get more responses to my question, it confirms what I thought. Hollow promises. I will try a triple chip to see if we get a better result.

6/19/15       #6: blade sharpenings ...
Mark V.

No way possible, at least in my experience and I am very careful in the set-up and maintenance of my equipment.

I have wondered if the diameter of the blade plays a roll in their longevity and that is why I mentioned the size of my saw blades. Smaller size = bad results ------ larger size = good results???

Which Holz-Her saw did you get and what is the blade size? I am assuming that it is a vertical panel saw because I don't think that I have ever heard of someone using hollow ground blades on a sliding panel saw.

Mark

6/19/15       #7: blade sharpenings ...
Cabmaker Member

Hi Mark,
It is a vertical saw, model 1254 250mm
diameter blade. Holzher specs the Leuco blade. As I said previously, I really just think this is more about salesman over promising. As you well know, there are so many factors when cutting on a vertical saw- Quality of melamine / core, cross cutting vs. ripping, 1 sheet at a time or 2, etc. I almost fell over when the Holzher salesman said 50 to 100 boards per blade. I have read similar threads on this site and most responses are very similar and even the best yield responses don't come anywhere close to 50 boards. I was surprised that a Holzher salesman would make a blanket statement like that. I needed to hear from others to confirm my sanity.

6/20/15       #8: blade sharpenings ...
Mark V.

Cabmaker,

I have to check, but I think that Leuco was what shipped on the Striebig as well. The weird thing was that while it was chipping on the frame side the exit side of the blade was clean. It was very frustrating….

I seem to recall someone saying that they were getting good life out of the hollow ground blades but I think they were using an Elcon vertical with 300mm blades, hence my statement about the size maybe making a difference. Different geometry, more teeth, runs cooler, angle of attack,etc. I don’t know… Maybe Bruce will chime in and let us know what size blades he is using.

The triple chip with reverse scoring for the odd piece or dropping the scoring blade when cutting a lot of important parts solved the problem for me, so I never researched it further.

Can you add the pre-scoring blades to you saw if you are not getting the results you desire?

Mark

6/25/15       #9: blade sharpenings ...
Jon Dieterlen Member

Although my experience with melamine is limited, I've ran a vertical saw for almost 30 years, cutting veneer core ply. I know PB core melamine will dull the blades faster than ply. I used those hollow ground blades in the beginning, but they do not stay sharp because of the fine point at the corners of the tips. They cannot disperse the heat created at the fine tips, thus they dull quickly.

I have had good luck with a high angle ATB with a 0 to -5 deg hook angle. I ran a Putch saw for years that had a 250mm blade. I think the tooth count was 80 for that blade. They lasted a long time cutting ply with no scoring. Triple chip blades do not work well with veneer core ply.

6/25/15       #10: blade sharpenings ...
Bruce H

I am use 300mm blade. I usually up score cut about a 1/6" deep before making the full plunge on the down stroke. On a Striebig you can set the riving knife to control the up cut depth.

7/1/15       #11: blade sharpenings ...
shawn

Website: http://activetooling.com

i have many customers that use a tcp or a atb grind with 2-5 deg. neg. hook works well cuts well TCP grind stays sharp the longest

7/2/15       #12: blade sharpenings ...
Cabmaker Member

I can't seem to find a TCG in a 250mm dia. / 30mm bore for the Holzher. Any help?

7/3/15       #13: blade sharpenings ...
Mark V.

Lots of manufacturers to choose from. My Striebig takes that blade size (with two additional pin holes) and I have never had a problem finding blades.

Google...
"250mm tcg 30mm bore saw blades"

or

Call your local reputable saw blade dealer/sharpener.

Mark

7/3/15       #14: blade sharpenings ...
Cabmaker Member

Thanks Mark
Found CMT 60TTCG for $65- less than half of what we're paying for Leuco and FS Tool hollow ground blades. Should also be cheaper to sharpen. Going to give it a try.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Excel Wood Products