Gluing teak together for outdoor table

3/28/24       
Mike

I have a customer who asked me for a price for an 1-3/4” top x 40” wide x 130” long.

What type of glue should I be using? I know Yellow blue isn’t going to work, but I think I remember seeing something about using a polyurethane glue. Or, could I use the same blue I use for doing veneer work which is a glue that has a catalyst powder

This will be an outdoor table, kind of like a picnic table.

Additionally, I was thinking of routing in flush, four or five pieces of 1/4” plate steel by about 2-3” wide x about 36-38” long and then screw it to the underside of the countertop to help prevent it from warping. I was also thinking of using SS threaded inserts with SS bolts (thoughts on this?)

She has the steel base legs that were powder coated. The base she bought was for a table out of white Oak that she bought on Etsy, but now wants me to provide a cost for a custom table base. I told her I think she’s going to need three bases to properly support it.

I explained to her that a film build finish is not going to be a good idea for an outdoor table, where a table can have a teak oil applied to it.

She’s kicking herself for believing the people on Etsy so now she’s stuck with this massive white oak table

3/28/24       #2: Gluing teak together for outdoor ta ...
RichC

Strips of steel are absolutely unnecessary, and even could be a rust problem outdoors. The strips of steel are merely an invention of fresh woodworkers on the internet. I've gone over 50 years of woodworking and have never put steel under a slab. According to makers today, I must be a magician. But in fact I just know how to build tables that won't warp.

3/28/24       #3: Gluing teak together for outdoor ta ...
duster

Epoxy would be the best glue for teak. But I wouldn't even consider gluing up a panel that large for an outdoor table. There's a reason why slat style tops, with a space between the boards is the usual solution. Expansion and contraction in solid wood panels is is a fact of life. An outdoor table is going to be subjected to way more swings in temperature and humidity than an indoor piece. It would be almost impossible to make a panel that large and expect it to hold up over the long term.

3/28/24       #4: Gluing teak together for outdoor ta ...
Matt Calnen

You most certainly can use metal to hold a top flat. I recommend “C” channel. [edited] There are times when metal channel strips are your only option, especially outdoors. Of course get something meant for the outdoor environment the piece will live in. Epoxy is the only glue I would use in this situation, as well as tongue and groove joints. Bid accordingly and bid high!

3/29/24       #5: Gluing teak together for outdoor ta ...
Chip Geffre

Mike-Resorcinol is the glue that I used for teak in marine applications.
It is waterproof and uv resistant.
Chip

3/29/24       #6: Gluing teak together for outdoor ta ...
Mike

To everyone who has replied…

[edited] If you don’t like someone’s idea, then let it go and move on. I just asked for opinions on my situation [edited]. If you can’t stick to the topic of answering my questions specifically, then please refrain from messaging at all on this thread.

This is exactly why I don’t participate in this group very often, because if I wanted drama in my life, I can easily find it by going on Facebook. This group is supposed to be comprised of professionals throughout the world with different levels and experiences, sharing it with the masses. We are all professionals and should act accordingly and if you can’t, please see yourself to the door. Thank you.

By the way, I have 30 years in the business this year and I completely understand why my topic got off track, but at the same time, people need to restrain themselves if they’re going to start cutting down others. What is good for the goose isn’t always good for the gander and people need to accept different ways will work effectively the same. I just don’t have a ton of experience in outdoor furniture, hence why I asked the question.

Thank you for playing along nicely in the sandbox

3/29/24       #7: Gluing teak together for outdoor ta ...
Gary

I second the notion of using resorcinol; epoxy has heat and UV limitations. If you want to build airplane propellors out of wood in Germany there is only one glue allowed.
Resorcinol.

3/30/24       #8: Gluing teak together for outdoor ta ...
Dave Edgerton  Member

I third the resorcinol method. Epoxy would be a close second choice if the dark colour of resorcinol is undesirable.

3/31/24       #9: Gluing teak together for outdoor ta ...
Hen Bob

Thanks for the tip on the Resorcinol glue, just ordered some. Always looking for better bonding options.

3/31/24       #10: Gluing teak together for outdoor ta ...
tom gardiner

If you go with epoxy I would recommend searching for a formulation specifically for oily woods such as teak. Doesn't mean standard West System will fail but there are better epoxies for teak.
UV degradation is not so much of a problem in glue lines as with surface finishes. The light penetration is very small.
Rich's point about constrained movement is a concern. Slotted fastener holes in the steel might be necessary depending on the climate. You can do a shrinkulator calculation from the resources above to check expansion. Slotting steel can get expensive if you don't have the equipment or friend in a machine shop. Wood battens are time tested and something you can produce in house whether sliding dovetail or slotted for screws.

4/1/24       #11: Gluing teak together for outdoor ta ...
Matt Calnen

The c channel I was referring to is readily available in many sizes at what I think are good prices. It comes made for wood tops, so they already have slotted holes.


View higher quality, full size image (750 X 1334)

4/2/24       #12: Gluing teak together for outdoor ta ...
Steve Member

Website: https://virmer.com/

Polyurethane glue would be a suitable option for outdoor use due to its water resistance and ability to bond various materials. Brands like Titebond Polyurethane Glue or Gorilla Glue Polyurethane would work well.

4/7/24       #13: Gluing teak together for outdoor ta ...
David R Sochar Member

Resorcinol Glue. Others glues may work, but Resorcinol is used to make wooden airplanes (Spruce Goose)
If you feel the need to have some sort of cross grain support, you can use wood or metal, as long as you allow for seasonal movement. Use the Srinkulator to determine how much the panel may move from season to season, and allow a bit more.
Remember the Two Basic Rules of Woodwork:
1. Wood will move
2. Woodworkers will forever disagree on the details.

5/14/24       #14: Gluing teak together for outdoor ta ...
Kustom Beams  Member

Website: https://kustombeams.com

For an outdoor table like this, you'll want to use a waterproof adhesive like polyurethane glue to ensure a strong bond that can withstand the elements. Avoid yellow or white glue, as they won't hold up well outdoors. The idea of using steel plates and stainless steel hardware to prevent warping sounds solid - it adds extra reinforcement. As for the table base, three bases would indeed provide better support for the size. Teak oil is a great choice for outdoor tables, offering protection and enhancing the wood's natural beauty. It sounds like you're on the right track!

8/15/24       #15: Gluing teak together for outdoor ta ...
Revel Woodard  Member

The slat idea is a good one, and not necessarily contrary to your query. Often times we are presented with an idea from a client, and gently steer them toward another one and the same vein that will serve them better. I find that is an integral part of woodworking in a professional capacity. Perhaps they are amenable to a slat design that will most likely make for a better and longer lasting product. I wouldn't use a polyurethane glue for a number of reasons, chief among them is that it degrades with UV exposure.

Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!