So there's been lots of discussion on this forum about cracked panels on exterior wood doors, and interesting ideas and methods to solve the problem. Apparently I need to pay closer attention. This is my first failure.

The question, then, becomes, has anyone had any success, or have a method, of fixing the cracks, aside from replacing the panel itself?

The door in question is 2-1/4" thick, with two 3/4" panels separated by rigid foam. The panels are held in by bolection moulding, so they can be removed if necessary. The panels are glued with TBII.

What I'm wondering about here is peoples successes or failures when it comes to field repair.

Thanks.


View higher quality, full size image (4032 X 3024)

4/3/24       #2: Fixing Panel Cracks ...
Fred

Website: http://www.rivercity.ca

Hi Christopher,

For glue joints in exterior door panel we had good luck with this glue.

https://www.richelieu.com/ca/en/category/glues-silicones-and-caulking/con
struction-glues-and-adhesives/polyurethane-glues/loctite-glue-ur-series/1209594 <
P>It can handle heat better. We found the Titebond just wont stand up in the direct sunlight of the Canadian prairie. My guess is heat and the resulting wood movement was to much for the glue joint.

4/3/24       #3: Fixing Panel Cracks ...
tom gardiner

I don't think will get a repair that will be satisfactory over time. You could fill and paint in a great stain match but that glue joint is prone to failure. My opinion is to spend the time and effort removing and replace/repair the panel. Bummer I know but it would be worse to have to do it a third time.
I guess the door is facing south or west.

4/7/24       #4: Fixing Panel Cracks ...
David R Sochar Member

After 35 years of dealing with the same problem you have, we determined that
1. There is no successful field repair other than replacement.
2. Titebond III glue is the worst glue ever foisted on the hapless woodworker.
3. 7 ply panels as detailed in my book "Small Shop Production of Custom Wood Doors" is the best and only solution.

4/8/24       #5: Fixing Panel Cracks ...
Christopher

Website: http://www.kalawood.com

Thanks for the replies and confirming what I already knew, lol.

Fred, thanks for commenting, you do beautiful work. In your process, what type of joinery do you use in combination with that glue? Unfortunately I wish I could blame heat and sun... the door has only seen one season so far, which was winter.

David, I have your book. I guess it's time to experiment with your process.

4/8/24       #6: Fixing Panel Cracks ...
Gary B.

Just a shot in the dark, but would it be possible to remove the panel, rip it with a thin kerf and reglue? a well-tuned bandsaw and a hand plane wouldn't remove much more than 3/32". Or maybe a thin kerf track saw?

4/8/24       #7: Fixing Panel Cracks ...
Christopher

Website: http://www.kalawood.com

Unfortunately I don't think that will work. Further evidence points to a larger problem, which leads me to believe that I'm looking at a process error. Most likely the wrong glue.

I'm not of the opinion that all the glue joints on a panel suffering from weather stress should be failing at the same time. You would think a stressed out panel would fail at one joint and then be relatively stress free? This panel appears to be failing all over.


View higher quality, full size image (3024 X 4032)

4/8/24       #8: Fixing Panel Cracks ...
David R Sochar Member

Two thin raises over a foam board is not sound. Make your panels "solid" and you can have a 3/4" tongue going into the moldings. This 3/4" or thicker is much stronger than thin wood with foam. Ditch da foam, my friend

4/8/24       #9: Fixing Panel Cracks ...
David R Sochar Member

Gary B- Rip and repair may be adequate for this panel this time. It does not address the real problem- how to avoid them altogether

4/8/24       #10: Fixing Panel Cracks ...
Fred

Hi Christopher,
We build panels up in several ways depending on style, grain, wood size and profile.
Also i do like David's way of building up the panels and I have his book as well. We have mostly done divided inner and outer panel. In our climate inside and outside temperature and conditions are often very different. The divided panels have worked better for us. But i believe as a manufacturer you have to adjust to what works best for you situation. Sometimes we add a layer of styro SM to get a higher R value.
As far as the Loctite glue goes we found it woks better on a clean sawcut than the moulder glue joint. Its messy to work with but its available in different open times. We had good results with it for exterior use.

4/10/24       #11: Fixing Panel Cracks ...
Joe Calhoon

On any exterior panels I never just use a straight glue joint. Normally I like a T&G joint or a shaped glue joint.
I have had pretty good luck with TB 3 but it is very inconsistent for viscosity and always stir the pails before use. It is rated D4 to withstand boiling water for a certain amount of time. I’ve tested in the past but believe given the inconsistency you may not always get the same results. I have been experimenting with a Jowat PVA that seems promising but to get a D4 rating on that an additive is needed and that gives a short pot life. For me that is a downside. The glue Fred mentioned looks promising. I also do 2 sided for planked panels but for raised panels I don’t like the thinness at the edge and prefer a single thicker panel for this. In my area flat plank panels are the norm except for historical work. The panels are usually not wide in historic doors so that helps.


View higher quality, full size image (3704 X 2778)


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!