Edgebanding glues: EVA vs Polyolefin

10/28/23       
Oggie  Member

I recently ran into a problem with my usual EVA glue—it just wouldn't stick to this one particular PVC edgebanding tape. So, I ordered a tape from a different manufacturer that matches the color, and I'm hoping it will do the trick when it arrives next week, but remains to be seen.

Right now, I'm not sure if the original tape was defective because it wasn't primed properly, or if it just didn't get along with my glue. I did some research, and it seems like stuff like this happens quite often, where the glue and tape don't play nice, even if neither of them is faulty.
In this particular case, the manufacturer of the PVC tape and board itself uses PUR glue for edge banding in their own production line, so maybe the tape in question was not primed at all, since PUR does not necessarily require primed tape (according to my google research).

I've been thinking, maybe switching to polyolefin glue could be a better option than sticking with EVA. My main goal is to avoid constantly switching between different glues and find one that works for most things. The problem is, there's not a lot of info out there about polyolefin glue.

So the questions:

1. Jowat 221 is one of the options suggested, but I'm curious if anyone here has any hands-on experience with it, or for that matter, any polyolefin glue?

2. What would be the pros and cons of polyolefin with regards to EVA?

3. Is there a way I could successfully apply primer to the unprimed PVC tape in some DIY fashion?

Thank you!

11/2/23       #4: Edgebanding glues: EVA vs Polyolefi ...
Bozzy Member

I almost asked the same question 3 weeks ago when we were getting ready to make the switch because I couldn't find anything on here about the PO. We have started using Jowat 237.5 unfilled PO glue and it seems to be going well so far. We've only used it with a walnut color laminate and can't tell right now if the glue line is thinner than EVA. One thing that I like is that we run it at 200C and it doesn't burn.

What I've been told about PO is that it sticks better than EVA and that it has better moisture resistance. The cost for us is about 50% more per bag than Jowat unfilled EVA, but if the performance is marginally better than EVA, I think it would be worth it. Will update once we have more experience

11/6/23       #5: Edgebanding glues: EVA vs Polyolefi ...
Oggie  Member

Thank you Bozzy.
I want to give it a try but can't find anyone who sells 237.50.
Guess I'll have to call Jowat directly tomorrow and see about that.
Where did you get yours (if you are in the US)?

11/6/23       #6: Edgebanding glues: EVA vs Polyolefi ...
Bozzy Member

I'm in Vancouver, Canada. I got it from Mckilican International. I would not use the Jowat 221 because it's not meant for edgebanding, but for wrapping.

We had bit of an issue when we started edganding 1" laminated plywood with PO last week. The tape wasn't sticking very well. I think the premill on our edgebander is getting a bit dull and was pulling some of the fibers out of the plywood that was perpendicular to premill and not allowing the glue to fully apply to the panel. This wasn't an issue with EVA because it's thicker than PO. We increased the the glue dosage from Dose 1 to Dose 2 and now the tape sticks perfectly. Need pliers to pull it off.

11/8/23       #7: Edgebanding glues: EVA vs Polyolefi ...
Oggie  Member

Took me almost a whole day to find out who has it in US.
Anyway, that 237.50 glue seems to be fairly new product on the market.
We should get it in a few days, I'm very eager to try it.

1/26/26       #8: Edgebanding glues: EVA vs Polyolefi ...
Pdub Member

Alright. It's been a couple years! what's your thoughts on the PO glue?


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Lamello
    Today's Sponsors
    • Safety Speed Manufacturing
      Economical Vertical Panel Saws, Panel Routers, Edgebanders and Widebelt Sanders
    • O'Shea Lumber Company
      Merchants of Fine Woods
    • Vacuum Pressing Systems, Inc.
      Vacuum Pressing Equipment - Including Bag and Frame Systems
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Original Saw Company
      Industrial Radial Arm Saws
    • Onsrud Cutter
      Router Tooling for Woodworking, Plastic and Non-Ferrous Metal Manufacturers
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • ULTI-BOARD
      The Ultimate Spoilboard - ULTI-BOARD - Specifically Engineered and Formulated for the Ultimate in Spoilboard Performance - Not Your Ordinary Sheet of MDF.
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • ETK International
      New and Used Woodworking Machinery, Spare Parts and Superior Service
    • GreCon
      Spark Detection and Extinguishment Systems and Quality Assurance Measuring Equipment
    • RT Machine Co.
      Stocking Distributor of New and Used Woodworking Machinery
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs

    Become a Sponsor today!