Subject: Re: Getting rid of pink color in alder

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Getting rid of pink color in alder

9/24/20       
Nick Cook Member

Website: http://kootenaicabinets.com

I'm trying to get a cappuccino color (light brown) on alder and I keep getting the pink or red coming back through when we add clear lacquer. I'm attempting this with a water base spray stain. Any good tricks for killing the red in clear alder. These are veneer slab doors from Northern Contours.

9/24/20       #2: Getting rid of pink color in alder ...
Leo G Member

Add some yellow-green dye to kill off the pink. Very small amount in the clear.

9/25/20       #3: Getting rid of pink color in alder ...
Nick Cook Member

Website: http://kootenaicabinets.com

Hi Leo,

Do you mean add it to the clear lacquer?

9/25/20       #4: Getting rid of pink color in alder ...
Leo G Member

Yes, that's what I meant. But in reality you might be able to add it to the stain too. If you do that it'd likely be a better experience all around. You won't have a odd tint to the clear. But it doesn't always work in the stain. It always works in the clear. Be sure not to over do it though in the clear or you'll see the cast of the color.

9/25/20       #5: Getting rid of pink color in alder ...
Nick Cook Member

Website: http://kootenaicabinets.com

Ok thanks Leo, I'll do some experimenting.

9/25/20       #6: Getting rid of pink color in alder ...
Shane Welch

Mohawk green dye M520 1/4 oz. of dye to 32 oz. of stain...... use a cup gun or pressure pot and make passes on the substrate to cover the panel evenly with this dye mixture.... This light mix should neutralize the perception of red poking through within one or two passes...strenthen or weaken the mixture as needed... then do your regular schedule of color..... samples samples samples!

9/27/20       #7: Getting rid of pink color in alder ...
Bart

I've done this a half dozen times on alder. I use GF's WB green dye heavily diluted with H2O and spray it on. Let it dry and then stain. Or you could seal with a spit coat/sand and then stain especially if it's a light or mid tone color you're looking for. Samples for sure.

my2cts

9/27/20       #8: Getting rid of pink color in alder ...
Shawn Turner  Member

Website: specializedfinishes.com

All of the responses above are solid solutions.

I am a fan of the yellow concentrated universal dye from Wurth or Sherwin mixed with whatever sealer I am using or just water, or lacquer thinner, about .5oz per gallon if-ish. You will be surprised at the results. some dyes look yellow but are leaning on the green side. So if something says yellow oxide expect it to lean red.

If you do not have dye available you can use tint. But, tint is made of particulate matter so it will often very subtly flatten your layers of color in wood grain to some degree.

Otherwise go OLD SCHOOL!!! XD

Oxalic acid, A&B Bleaches, homeowner wood brighteners.

Follow those direction and do not get it on anything you do not get it on or in your skin, eyes, mouth yadda yadda. Follow all safety precaution that will be found on the back of the product container.

Once again my disclaimer. There are other dyes available on the market.

I am not pushing Wurth Lewis or M.L. Campbell one bit. Do not get me started about Sherwin Williams.

Compare products and try to buy locally if possible. ALWAYS!

Always read the back of the can!


View larger image

Woodsong II Microton Spray Dye Stain

9/28/20       #10: Getting rid of pink color in alder ...
Shane Welch

I messed up my suggested formula.. I meant 1/4 oz. of green mohawk M520 to 32oz. of acetone... Several even passes of this weak mixture on raw wood will shift the color enough to be workable. Lemon yellow could also be a mohawk option as it it a yellow/green.... we use this technique a lot to even out substrates to the same playing field before we go into regular stain procedures.... taking care of sap lines... differences in varied color...(using different colors as necessary) get it fairly even at the raw wood stage and then proceed to bring the main color up to snuff...

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Carter Products
      Band Saw Guides, Blades, Wheels, Tires, Line Lasers and 2D Projectors, Wide Belt Sanding Accessories, Vacuum Holding Systems and More
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs

    Become a Sponsor today!