Subject: Re: CV mixing by volume or weight ?

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

CV mixing by volume or weight ?

10/26/20       
Tom Gafgen

Do most of you mix by volume or by weight ? I've been mixing by volume for 20 years with never a problem but have recently switched to a new type of pail liner to mix in which is making it difficult to read my measuring marks on the pail accurately .So I am considering switching to the weight method which I'm sure is dead on accurate and I guess my question should be How accurate does the 10%catylst ratio have to be ?Would being off by 1% either way cause noticeable problems ?

10/26/20       #2: CV mixing by volume or weight ? ...
gralyn Member

what we did is cut a slot into a sacrificial pail vertical that will act like a window to see the liner. leave the pails rim intact . add your graduation marks on the pail. This option has worked well for me.

10/26/20       #3: CV mixing by volume or weight ? ...
Jim Clark  Member

It doesn't have to be that accurate.
I have varied mine a lot depending on
the temperature.

10/26/20       #4: CV mixing by volume or weight ? ...
Jim Clark  Member

Most measuring cups aren't that accurate either, in fact some are quite a bit off.

10/26/20       #5: CV mixing by volume or weight ? ...
Shane Welch

we use pail liners to mix quickly for less than 5 gal. batches.... We made stir sticks from aluminum bar with graduated lines on the stir stick to reference how much material is poured into the liner... marks at 1 gal, 2 gal, 2.5 gal, 3 gal etc etc... strain and pour material up to the line... then we always measure catalyst in a small graduated plastic mixing tubs we have handy and just give them a little rinse .. that way at least the catalyst is measured fairly close... Quick n easy

10/26/20       #6: CV mixing by volume or weight ? ...
DannyB Member

Mixing large amounts by weight is a pain in the ass for a number of reasons.

Like others, i wouldn't bother.

Acid-cured CV is not particularly sensitive about catalyst.
The main issue if you add too much is you'll end up with white particles in the finish - this is the catalyst that is not used up.

The only thing i mix by weight is small batches of stuff that is more sensitive to catalyst amount.

10/27/20       #7: CV mixing by volume or weight ? ...
Tom Gafgen

Thanks for the responses and good ideas and also for confirming that there's no reason to switch to the weight method , I think that would have been a pain .

10/27/20       #8: CV mixing by volume or weight ? ...
Shane Welch

not to mention a scale that can handle that sort of weight accurately is $3k... lol.. I know.. We have one for mixing paint colors with Sherwin's tint system for opticolor...

10/27/20       #9: CV mixing by volume or weight ? ...
DannyB Member

I was actually just gonna say that - a nice accurate scale for that is thousands, and good luck getting one that is meant to be around lots of solvents.

11/10/20       #10: CV mixing by volume or weight ? ...
Y.Heller Member

Buy scientific lab graduated cylinders for the catalyst.

Plastic cylinders read straight across the graduated line while glass reads to the bottom curve of the meniscus. There can be a degree of error in that reading based on your viewing angle of that curve/ who’s looking at it and what they read it as. And obviously the plastic ones are far more durable than the glass.

The plastic cylinders come in different types. There is PPCO which is a cloudy clear plastic and PMP which is entirely clear like glass. For highest accuracy you’re looking for Class A bit they also come in Class B which has a higher degree of error.

The Class A are somewhere around $20.00.

11/10/20       #11: CV mixing by volume or weight ? ...
Y.Heller Member

Correction. They’re around $40-45 for a 500ml (16oz). Price vary by size.

12/22/20       #12: CV mixing by volume or weight ? ...
Jim

Y Heller
That sounds very good. So where you go to purchase?

Thanks !

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations

    Become a Sponsor today!