Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Sanded through veneer

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Sanded through veneer

6/19/23       
Adam Clark Member

Using white oak (flat/plain sawn) sheet goods and edge joining to make large panels. I sanded through the veneer slightly in two spots (different thickness on sheets for mfg.). What's the best approach to fix? Thanks!

6/19/23       #2: Sanded through veneer ...
Leo G Member

There probably isn't a best way to fix it. Depending on how big the spots are you might be able to do some faux painting to hide it.

Very doubtful you can cut in a new veneer pc but it is possible. Find something with the correct graining and cut it in, glue it and sand it. Pretty difficult.

Remake the part is the likely fix.

6/19/23       #3: Sanded through veneer ...
RichC

Best way to fix is scrap that and start over. You want to provide the best possible result to your customers and the cost of a couple of sheets of plywood is not even a questionable decision to sell a patched up panel. There is no slightly when it comes to sanding through. You either did, or you didn't. Also seek out a better plywood supplier. You surely aren't buying big box store import plywood are you?

6/20/23       #4: Sanded through veneer ...
Adam Clark Member

Unfortunately, it's not as simple as using new pieces. It's a sequenced elevation and I purchased 10 sheets from the same unit from one of my area's better hardwood suppliers. Out of the 10, I carefully laid out 6 that matched very well. This joint is a small seem that I couldn't avoid and I have to roll with it. I'm going to cut it apart and re-join it with the domino and hope for better face alignment. The back is hidden. If it happens again, I'll need a solution.

6/20/23       #5: Sanded through veneer ...
D Brown

To repair it take a straight edge and a router with a straight cutting bit , make the cut maybe an 1/8" deep, I have used a small piece of solid stock that matches closely, This way you can size it perfectly to avoid much sanding.

Good luck,, " how good you are is how good you fix your mistakes"

6/20/23       #6: Sanded through veneer ...
RichC

Using a piece of solid stock to repair veneer will cause the solid stock to stick out like a sore thumb! Veneer is sliced wet and the absorption of finish is quite different than solid stock. It would still take a magician finisher to get it to blend in. Next time, use a card scraper to flush up the plywood surfaces. I'd also suggest a spline to line up the sheets. I use a slot cutter on the router and it lines up better than any other method of joinery.

6/20/23       #7: Sanded through veneer ...
Tom Gardiner

If you still have the width recut the joint removing the sand through. Careful re-glue with domino or biscuits (if you trust your biscuit joiner)

6/20/23       #8: Sanded through veneer ...
D Brown

Rich, solid stock next to veneer happens all the time when a face frame butts to a finished end so it not unusual.With care Oak is easy to splice and match grain.He did say the back is hidden.

6/21/23       #9: Sanded through veneer ...
chemmy

Is this project one with a natural finish, or are you staying or dying it.?

6/21/23       #10: Sanded through veneer ...
chemmy

Is this project one with a natural finish, or are you staining or dying it.?

6/21/23       #11: Sanded through veneer ...
kevin

This is timely!! I drilled a cup hinge hole through a sequenced veneer door on the show side today, great day in the shop!!!

6/21/23       #12: Sanded through veneer ...
Leo G Member

I did that a long time ago. I was able to find a pc that was very close and I replaced the door. No one said anything. I doubt they noticed. I had a hard time seeing it and I was the one who did it.

The stop on my drill press jumped thread and I pushed right through the door. Boy did some nasty words come out of me.

6/21/23       #13: Sanded through veneer ...
RichC

D Brown,
Sure solid butts up to plywood all the time, but not in the middle of a panel. The two materials never match perfectly when the finish goes on.

6/22/23       #14: Sanded through veneer ...
Adam Clark Member

The finish is going to be "natural," so no stain. I was able to cut it apart and rejoin with the domino and got much better results. Side note, the domino is great you just have to go SLOW. The BACKS are still an issue as the ply varies in thickness a bit. Not that worried about these, but I am going to experiment with Konig's "Paint Box" kit to faux it in.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products

    Become a Sponsor today!