2/15/21       
David Waldmann Member

Website: vermonthardwoods.com

We are a relatively small picture frame moulding manufacturer/distributor. We have a series of catalog mouldings that are milled and stocked raw, then finished to order. We also offer custom profiles/finishes, which would be milled to order, then finished.

We have 42 stock profiles, and 47 different wood/finish combinations. So we are often finishing 5-10-20 feet of a particular item.

However, we also have several items that are popular, and we may end up finishing 25-50 feet of those every day, or get individual orders for 100-200-500-1000 LF. We have also gotten quote requests for 1000-5000 feet that we just cannot be competitive on.

We are considering making the jump to an automated lineal spray system, so we can run several hundred feet at a time of the popular items, as well as these larger individual/custom jobs.

However, it's more than a "jump" - more like an Evil Knievel attempt across the Grand Canyon. The machine we're looking most seriously at is a Cefla PSP-6, and like most machines of that type it's capable of 100-150 LF per minute, or orders of magnitude more than we can do by hand.

Between the spray machine itself, air make-up, pumps and guns, the cost to partition off the space, drying racks and things I don't don't know plus those things I don't know I don't know, we are looking at at least $100k, probably $125k.

Pretty big leap. Am I missing a step-stone?

2/15/21       #2: Medium volume lineal spray finishin ...
herb johnson

i am not sure of your widths and i don't know your drying profile, nor your color changes per day etc, but have you looked at an MM150 in the 25-30k range

good luck
herb j

2/15/21       #3: Medium volume lineal spray finishin ...
Chris

I have an older version of a MM150. We use it for spraying dye stain on frame moldings.
It works ok but changing between colors is a pain. Also if spraying sealer or topcoat it gets messy

2/16/21       #4: Medium volume lineal spray finishin ...
David Waldmann Member

Website: vermonthardwoods.com

Our profiles are mostly in the 1-2" wide range. I wouldn't envision doing more than one or two fluid changes per day. Our typical dry time ranges from 30 minutes to 2 hours depending on coating (all water-based), temp and humidity.

Thanks,
David

2/16/21       #5: Medium volume lineal spray finishin ...
rescraft

Just Googling, one for sale that says it's almost new $81k. I'm sure there are other deals out there. Good luck.

2/16/21       #6: Medium volume lineal spray finishin ...
herb johnson

honestly i am far from an expert in automated finished of mouldings etc i just responded to the question of is their anything else out there, based on what you said, their is a step in the middle , an mm150 type machine, there are a lot of machine mfg's that make this type of machine, it is quite basic with three or four heads, one or two, have seen three fluid circuits, a whisker or limit trigger switch to actuate the guns, you place the machine infront of a spray booth, it is a work horse. i would suggest you investigate to see if meets your needs, it wouldn't make sense to run it for 15ft, etc but it might fit your needs, there are videos of this "type " of machine on you tube. as far as drying the part, you could get a prime heat oven which will do a great job on curing w/b coatings and will be well under the threshold ur were budgeting for the cefla machine
good luck
herb j

2/16/21       #7: Medium volume lineal spray finishin ...
David Waldmann Member

Website: vermonthardwoods.com

We can't set it in front of our spray booth, there just isn't room.

However I do see that the MM150 machine is available with a hood and fan, and only requires a 120v 1Ph power source, which would be an advantage.

I am waiting for a quote from another supplier for this type of machine. I am, however, concerned with another posters' comment that "...changing between colors is a pain. Also if spraying sealer or topcoat it gets messy".

2/16/21       #8: Medium volume lineal spray finishin ...
herb johnson

if you get a machine with air assisted airless that is your best bet, don't get a machine with hvlp it will be a nightmare.

also get acrastrip for your colorchanges

2/16/21       #9: Medium volume lineal spray finishin ...
Chris

We originally had our machine set up. With AAA but couldn’t get it to work right for spraying dye stain so we switched to hvlp.
Spraying water base would probably work a lot better

2/16/21       #10: Medium volume lineal spray finishin ...
herb johnson

with dye stain the iwata gun with the tulip nozzle is killer set up , so a two circuit machine is the way to go, one diagphram pump system with t;he iwata guns with the tulip nozzles and the an aa system with 15 or 20-1 set up with say a 1 gpm delivery and you will have terrific set up

2/19/21       #11: Medium volume lineal spray finishin ...
JeffA

In my opinion you need to keep all the staining by hand and do the clear coating on the automated sprayer. And it's more important how many different widths of product you have as the automated sprayer is dictated by that. 3 guns on it should be more than good enough if the largest width is only 2 inches.
I wouldn't even think of doing any staining on the machine unless it's a pigmented product and you run 1000's of linear feet at a time. 47 colors are just way too many for an automated line unless you learn to stock finished product which now a days owners hate to do. ;.)


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Carter Products
      Band Saw Guides, Blades, Wheels, Tires, Line Lasers and 2D Projectors, Wide Belt Sanding Accessories, Vacuum Holding Systems and More
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs

    Become a Sponsor today!