Subject: Re: Veneering Solid Wood

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Veneering Solid Wood

6/7/23       
Derek Member

The veneer will be 1/8 - 3/32 thick and I was planning on just veneering 1 side of the teak panels. However, during my research I found a lot of people saying that you need to veneer both sides of your substrate. But in every example they were veneering some sort of plywood.

Does anyone have experience veneering Solid wood and is it necessary to veneer both sides?
6/8/23       #2: Veneering Solid Wood ...
Tom Gardiner

I have veneered a single face of solid wood. They were small pieces - speaker faces, the veneer was 1/42" and the panel was 1 1/8" thick. The grain ran the same direction for both veneer and substrate. It was a low risk scenario and there were no issues.
I would not do this if the panel size is large, the grain direction is opposite to one another or if the veneer is as thick as you are planning. The thicker the veneer, the more force it can impart on the panel. If you use a glue with water as a component then you will be adhering a swollen veneer skin to one side of the panel. Once the glue is set and the moisture evaporates the veneered side will shrink and warp the panel. How much will depend on the ratio of thickness of veneer to substrate, the moisture added and the species and cut of the veneer.
You can use epoxy or polyurethane glue to not add moisture and opt veneer that matches the grain orientation and cut of the substrate to minimize the risk. It will likely stay flat out of the press, however, there may be issues in the future as the panel might react to environmental moisture deferentially from face to back and cause warping. Is this a project you can experiment with? I wouldn't want to deliver a piece to a customer without being sure it will stay flat over time.

6/8/23       #3: Veneering Solid Wood ...
Derek Member

Thanks for your input Tom. Makes sense on the veneer thickness and the other points you mentioned. The grain will be oriented the same, I will opt for epoxy on the glue up, and I have room to decrease the veneer thickness. I'm choosing teak for the substrate as it is a very stable wood. I have kiln dried both the veneer material and the teak and everything is metering at EMC.

I will also mention that I am using rift and quartersawn substrate.

6/8/23       #4: Veneering Solid Wood ...
Tom Gardiner

One last thing. If you are going to use epoxy for the veneer I suggest you coat the back with epoxy, if possible, to balance the environmental moisture absorbtion of the two faces.

6/8/23       #5: Veneering Solid Wood ...
Derek Member

Tom,

Let me see if I understand you. My plan was to use an oil based hard wax, Odie's oil, finish on the front and interior. Your suggestion is to finish the back of the panel in epoxy If I use epoxy as my adhesive for the veneer strips?

Is this to help even the moisture movement in the teak substrate?

6/8/23       #6: Veneering Solid Wood ...
Tom Gardiner

Yes that is my theory. When you epoxy the face veneer it becomes a moisture barrier so the other face might absorb moisture more quickly without epoxy. Rift teak is very stable so you may be able to ignore this step. How much humidity swing is there annually in your projects location? There is a wood movement calculator on this website so you can check what you might expect with seasonal change.
I don't use epoxy much but you want to check about which epoxies are compatible with oily woods. Seem to recall there being formulations for oily wood

6/10/23       #7: Veneering Solid Wood ...
Derek Member

Tom,

Humidity fluctuates between 65% and 90%. And about 86 degrees all year round. So yes pretty humid. After careful deliberation, your advice and the movement calculator I have decided to track down some mdf for the substrate.

My new plan is 1/16 inch spalted tamarind veneer epoxied to mdf front and back. More time but seems like this is the best route for long term success. I understand that the mdf surface should be sanded with 80 grit to creat a surface suited for the epoxy to grip onto?

I don't have a vacuum press but I did aquire two broken pieces of granite larger than the door sizes to act as my press. I plan to use wax paper and scotch painters tape to hold the veneer and keep the epoxy from adhering to the granite.

If you think of anything I am missing please let me know. Thanks again for your advice.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!