Veneer

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Maple Burl Veneer Table Tops

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Maple Burl Veneer Table Tops

4/17/24       
vince

Preparing to build tables as shown in photos.

The tops are planned to be raw maple burl veneer over 2 layers of 3/4" MDF face glued together with a 4 to 5 inch wide solid white oak frame.

Am I good with just the raw maple veneer only, since the table top will be 1 1/2" thick with the heavy frame?

Or is it neccesary to apply another layer of veneer (Sapele?) either between the MDF sheets, or on the bottom of them?


View higher quality, full size image (1078 X 545)

4/18/24       #2: Maple Burl Veneer Table Tops ...
David

The maple burl veneer should be two plied for stability. Just using the veneer single ply is a recipe for disaster.

4/18/24       #3: Maple Burl Veneer Table Tops ...
Vince Member

I am assuming you mean a of layer of standard maple veneer on the bottom? Hopefully it does not need to be burl like the top?

4/18/24       #4: Maple Burl Veneer Table Tops ...
David

Vince,

I’m not sure where you’re located, but I would try to find a veneer face shop that can two ply these faces. Plain maple for the backer would be fine. A face maker would sandwich a glue film between the two veneers and then press them together. Essentially you would have one thick veneer face once it’s completed.

4/19/24       #5: Maple Burl Veneer Table Tops ...
Vince Member

I am all ready to adhere the veneer to my substrate with vacuum bags and cauls anyway.. why can't I two-ply the face veneer in my shop if that is truly what is required for this project?

Also, can someone explain why I cannot just flatten and then glue this quad-matched maple burl 1 ply?

4/19/24       #6: Maple Burl Veneer Table Tops ...
John Costin

YMMV, as they say on the message boards, but custom veneer has been our core business for almost 25 years so our practices are pretty well road-tested. Here goes.

The logic of making a balanced panel (veneered both sides, more on that in a moment) is that veneer is wood. As such, it will expand and contract across the grain with changes in moisture content. We see those changes seasonally, when moving environments, and as moisture leaves or enters the panel from adhesives, finishes, etc... In a balanced panel, both faces will expand or contract relatively equally; because equal force is exerted on both sides, the panel should stay relatively flat even when the MC of the faces changes. If only one side expands or contracts the panel may warp.

Sometimes people get away with veneering only one side of a panel. A very rigid panel may be able to resist the force of the expanding or contracting veneer. But wood can be strong -- think about how stone was traditionally quarried by inserting very dry wood pegs into holes in the stone, then pouring water on them; the force of the expanding wood is enough to shear huge masses of stone. You might be surprised by how thick of a panel can be warped by one-sided veneering.

By this explanation you can see that the choice of balancing veneer can be important. Often, panel mills will balance semi-custom panels with inexpensive rotary tropical veneer where the backs will not be seen. This has led many woodworkers to think that the balancing veneer is not important and that any backer will work. This is not always the case, and in fact the Architectural Woodwork Institute specifies that balancing veneer should be as similar as possible to the veneer on the show face.

We really see this with burl veneer. Because of the way burls grow, burl wood expands and contracts in all directions (there is no "across the grain" with burl). So if we balance a burl panel with longwood we are only balancing it in one direction. If the panel is able to warp, it will. For this reason, we usually use a less-expensive burl veneer to balance where backs/bottoms will not be seen. Sometimes synthetic sheets (Gatorply, Yorkite, etc...) can be used because these will also expand and contract in all directions.

As for crossbanding (applying veneer between the veneer and the panel) I don't think it's necessary in the case of burl. It is often used with crotch veneer because crotch is very brittle and has a tendency to shatter along the grain lines. In this case, a longwood crossband running perpendicular to the crotch can help restrain movement of the crotch veneer. When adhering a burl veneer to MDF you actually have a very friendly condition: both the substrate and the veneer are expanding and contracting in all directions. We have never seen problems with crotch veneer pressed directly to MDF with an appropriate adhesive.

I hope that this information is helpful to you, and good luck!

John Costin
Veneer Services Unlimited
Custom Veneered Products for the Woodworking Industry
(207) 459-7221
vsu@gwi.net

4/20/24       #8: Maple Burl Veneer Table Tops ...
Joseph Eultgen

Call Indiana Architectural veneer in trafalgar Indiana. Ask for Steve Stanton. They can make you up the veneer glued to your core and thickness if choice ir they can make you ply faces. 2 or 3 y faces. The work they do us Incredible and very fairly priced.

4/21/24       #9: Maple Burl Veneer Table Tops ...
John Costin

I just caught a typo in my post above. I should have written "We have never seen problems with *burl* veneer pressed directly to MDF with an appropriate adhesive."

My apologies if this caused any confusion.

John Costin
Veneer Services Unlimited
Custom Veneered Products for the Woodworking Industry
(207) 459-7221
vsu@gwi.net

4/23/24       #10: Maple Burl Veneer Table Tops ...
vince

John,

Thank you for your detailed response. Plan is to adhere the maple burl veneer directly to MDF surface, with another sheet of maple burl on the bottom as well. Would it be ok to pick a less figured maple burl for bottom?

Planning on using this glue: https://www.veneersupplies.com/products/Better-Bond-X-Press-Veneer-Glue.html

My
plywood supplier will not do small amounts of high density MDF, but they do offer a veneer core with mdf on outer layers. I am assuming this is alright to use in place of solid MDF?

4/23/24       #11: Maple Burl Veneer Table Tops ...
John Costin

Vince --

Using a less-precious Maple burl veneer on the bottom of your table is a good move.

Veneer core with MDF outer layers (PLUMA HDF is dominant in the market, I believe) is a good substrate, too. Sometimes that MDF face is little mill-glazed; a light scuffing is cheap insurance for adhesion.

Lastly, I don't have any direct experience with the adhesive you referenced but I believe it is a PVAc-based glue. It should be fine, and your options are pretty limited at this point due to EPA regulations on urea-formaldehyde trickling down to small shops effective at the beginning of this month.

John

John Costin
Veneer Services Unlimited
Custom Veneered Products for the Woodworking Industry
(207) 459-7221
vsu@gwi.net

4/23/24       #12: Maple Burl Veneer Table Tops ...
RichC

I'd be more worried about any wide miters on the frame and that extreme overhang on the left table.

4/24/24       #13: Maple Burl Veneer Table Tops ...
Vince Member

Rich C-

Do you think butt joints would be better than miters for the white oak frame?

All overhangs are the same, must be optical illusion that one table has more. They wanted plenty of space for legs under tables.

Anyone else-

Is red rosin paper acceptable for stacking between the softener-wetted veneers in the drying process? I want to avoid any possible staining from this part of the process.

4/24/24       #14: Maple Burl Veneer Table Tops ...
John Costin

I haven't tried rosin paper but I would not use it based on the fact that it is intended to be a moisture barrier. You want something that absorbs moisture. Plain brown kraft paper is great -- try to find the stuff that is most like an old school paper grocery bag (you could even use old school paper grocery bags if your veneer leaves are small enough). We see this as dunnage in packages often.

HDF or MDF will also work. Avoid anything that is treated, like tempered hardboard. You want the moisture from the veneer flattener/softener to be absorbed into the stacking material.

John Costin
Veneer Services Unlimited
Custom Veneered Products for the Woodworking Industry
(207) 459-7221
vsu@gwi.net

4/24/24       #15: Maple Burl Veneer Table Tops ...
Vince Member

I found this:

https://www.amazon.com/PerkHomy-Wrapping-Bulletin-Shipping-Covering/dp/B0
CQZ1TYX9/ref=mp_s_a_1_2_sspa?crid=2OYH4NBTDYUU&dib=eyJ2IjoiMSJ9.sZoU0DkxYkz1V
3QjQ5ldDsoqMZgtjV65eqBqoKuIAl8ecJfXo2_w2-A4oC-HWg1TyKwR0RD9GQwSENR6dCeumoiK-AQJgo
QcTvt5sSX-5xxlmlm7rB3FufIaQgtwxyzkQnatsZPCLW5d2lmSlYVdZlZ5yhSQomFnyyfbgMjWLjxTV3Y
qOEdBnDDnJ7SKrHYPuouxheWSux-9KiSKfXcMWw.ird_wYr0HejeGvNEwBW-8E3J7A3nMv7uE2GqXpvmE
uM&dib_tag=se&keywords=brown+kraft+paper+roll&qid=1713973254&spre
fix=brown+kraft+%2Caps%2C207&sr=8-2-spons&sp_csd=d2lkZ2V0TmFtZT1zcF9waG9u
ZV9zZWFyY2hfYXRm&psc=1

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!